View clinical trials related to Mineral Trioxide Aggregate.
Filter by:The aim of this study was to determine the subcutaneous connective tissue reactions to these new materials. Materials and Methods These materials were placed in polyethylene tubes and implanted into the dorsal connective tissue of Sprague Dawley rats. The presence of inflammation, edema, necrosis, dystrophic calcification, and thickness of fibrous capsule formation was recorded by histological examination 7, 30, and 60 days after the implantation procedure. Inflammation scores were defined as follows: 0 = no or few inflammatory cells, no reaction, 1 = <25 cells, mild reaction; 2 = 25 to 125 cells, moderate reaction; and 3 = ≥125 cells, severe reaction. Fibrous capsule thickness, necrosis, and formation of calcification were recorded.